Just wondering what the concensus if any for the thinning of MM acrylics. I tried using rubbing alchol and the weekend, and the results were less than favourable. I use rubbing alchol for Tamiya paints and future with good results.
Thanks in advance for your input
Ted
AFV Painting & Weathering
Answers to questions about the right paint scheme or tips for the right effect.
Answers to questions about the right paint scheme or tips for the right effect.
Hosted by Darren Baker, Matthew Toms
MM acrylics - thinner?
klimmer
Ontario, Canada
Joined: May 16, 2003
KitMaker: 250 posts
Armorama: 36 posts
Joined: May 16, 2003
KitMaker: 250 posts
Armorama: 36 posts
Posted: Tuesday, February 21, 2006 - 10:50 PM UTC
AJLaFleche
Massachusetts, United States
Joined: May 05, 2002
KitMaker: 8,074 posts
Armorama: 3,293 posts
Joined: May 05, 2002
KitMaker: 8,074 posts
Armorama: 3,293 posts
Posted: Tuesday, February 21, 2006 - 10:55 PM UTC
H2O.
Posted: Tuesday, February 21, 2006 - 11:15 PM UTC
I use distilled H20
klimmer
Ontario, Canada
Joined: May 16, 2003
KitMaker: 250 posts
Armorama: 36 posts
Joined: May 16, 2003
KitMaker: 250 posts
Armorama: 36 posts
Posted: Thursday, February 23, 2006 - 07:54 PM UTC
Thanks guys. Never in the world would have thought it was that simple.
propboy44256
Ohio, United States
Joined: November 20, 2002
KitMaker: 1,038 posts
Armorama: 454 posts
Joined: November 20, 2002
KitMaker: 1,038 posts
Armorama: 454 posts
Posted: Thursday, February 23, 2006 - 09:39 PM UTC
I use rubbing alcohol, it works, but need to mix and mix and mix very well.